Fushun Inconel Alloy 625 Nickel Based Superalloy Round Bar

Catégorie:

La description

Fushun Inconel Alloy 625 Nickel Based Superalloy Round Bar

Information produit
Introduce
Inconel 625 has excellent strength at temperatures up to 816℃. At higher temperatures, its strength is generally lower than that of other solid solution strengthened alloys. Inconel 625 has good oxidation resistance at temperatures up to 980℃ and shows good resistance to aqueous corrosion, but is relatively moderate compared to other more capable corrosion resistant alloys.

Application
Chemical process industry and sea water application. Inconel 625 is used in short term applications at temperatures up to 816℃. For long term service, it is best restricted to a maximum of 593℃, because long term exposure above 593℃ will result in significant embrittlement.

Grade Comparison
AMS: 5599, 5666, MS: 5837, COMME MOI: SB 443 Gr 1, SB 446 Gr 1, ASTM: B 443 Gr 1, B 446 Gr 1, EN: 2.4856, ISO: 15156-3, NACE: MR0175-3, UNS: N06625, Werkstoff: 2.4856

Cr
Mo
Co
Nb+Ta
Al
Ti
C
Fe
Mn
Ni
20-23
8-10
1
3.15-4.15
0.4
0.4
0.1
5
0.5
Équilibre
Condition
Formulaire
Ultimate
Tensile
Force,
ksi (MPa)
Yield
Force
à 0.2%
offset,ksi (MPa)
Elongation
in 2
pour cent
Dureté,
Rockwell
Annealed at
1925°F (1052°C),
rapid cooled
Sheet 0.014-0.063″ épais
132.0 (910)
67.9 (468)
47
B94
Annealed at
1925°F (1052°C),
rapid cooled
Sheet,0.0.78-0.155″ épais
131.5 (907)
67.4 (465)
45
B97
Annealed at
1925°F (1052°C),
rapid cooled
Plate,
1/4″
1/2″
3/4″
1.00″
1-1/2″
1-3/4″
132.0 (910)
130.0 (896)
132.3 (912)
127.2 (877)
127.3 (878)
128.0 (883)
65.5 (452)
67.0 (462)
80.0 (552)
75.3 (519)
73.7 (508)
66.0 (455)
46
44
44
42
43
44
B94
B98
B98
B97
B97
C20
Spring Temper
1250 1500
180 225
Non 1 Caractère + Annealed + Aged
1250 1450
181 210
-200 à +550
-330 à +1020
Non 1 Caractère + Aged
1520 1720
220 250
Contact Alloy Wire Technical Dept
Spring Temper + Annealed + Aged
1250 1450
181 210
-200 à +550
-330 à +1020
Spring Temper + Aged
1700 1950
247 283
Contact Alloy Wire Technical Dept
Heat Treatment
Alloy 625 has three basic heat treatments:
(1)High Solution Anneal – 2000/2200°F (1093/1204°C), air quench or faster.
(2)Low Solution Anneal – 1700/1900°F (927/1038°C), air quench or faster.
(3)Stress Relieve – 1650°F (899°C), air quench.
The time at the above temperatures depends on volume and section thickness. Strip, par exemple, would require shorter times than large sections. Temperatures for treatments No. 1 et 2 are generally held for 1/2 à 1 hour, 1 à 4 hours for treatment No. 3. Treatment No. 1 is not commonly used for applications below 1500°F (816°C). It is generally used above 1500°F and where resistance to creep is important. The high solution anneal is also used to develop the maximum softness for mild processing operations such as cold rolling or drawing.
Treatment No. 2 is the used treatment and develops an optimum combination of tensile and rupture properties from ambient temperatures to 1900°F (1038°C). Ductility and toughness at cryogenic temperatures are also very good.
Treatment No. 3 is recommended for application below 1200°F (649°C) when maximum fatigue, hardness, tensile and yield strength properties are desired. Ductility and toughness at cryogenic temperatures are excellent. When a fine grain size is desired for fatigue, tensile and yield strengths up to 1500°F (816°C), treatment No. 3 is sometimes used.

Hot Working
Hot working may done at 2100°F (1149°C) maximum furnace temperature. Care should be exercised to avoid frictional heat build-up which can result in overheating, exceeding 2100°F (1149°C). Alloy 625 becomes very stiff at temperatures below 1850°F (1010°C).
Work pieces that fall below this temperature should be reheated. Uniform reductions are recommended to avoid the formation of a duplex grain structure. Approximately 15/20% reduction is recommended for finishing.

Cold Forming
Alloy 625 can be cold formed by standards methods. When the material becomes too stiff from cold working, ductility can be restored by process anneal.

Machineability
Low cutting speeds, rigid tools and work piece, heavy equipment, ample coolant and positive feeds are general recommendations.

Corrosion Resistance
Alloy 625 has withstood many corrosive environments. In alkaline, salt water, fresh water, neutral salts, and in the air, almost no attack occurs. The nickel and chromium provide resistance to oxidizing environments. Nickel and molybdenum provide for resistance to nonoxidizing atmospheres. Pitting and crevice corrosion are prevented by molybdenum. Niobium stabilizes the alloy against sensitization during welding. Chloride stress-corrosion cracking resistance is excellent. The alloy resists scaling and oxidation at high temperatures.

Pickling
Sodium hydride baths are necessary to descale this alloy. After the sodium hydride treatment, the material should be immersed in a sulfuric acid bath 165°F (74°C) for approximately 3 minutes. A 25-minute immersion in a nitric-hydrofluoric bath 145°F (63°C) is then necessary. Rinse. Sulfuric solution: 16% by weight, H2SO4. Nitric solution: 8% HNO3 by weight and 3% HF by weight. Acid etching for macro-inspection-expose material electrolytically to a 3-to-1 HCl to HNO3 solution, saturated with CuCl2 at a current density of 0.645 amp/in² (25.4 A/m)

Produce Process
Factory Information
Recommander des produits

FAQ

1, What is your time of making a sample?

Usually we will take 1~3 days to make the sample

2, Quel est votre MOQ?
1-3 tons accordingto different size for stocks.

3,Quel est votre délai de livraison?
For stocks, we can send the goods to loading port within 7 days after receiving your deposit For production period, it usually needs about 15days- 30 jours après réception du dépôt

4, What is your shipping port?
Tian jin port, Qingdao port, Port de Shanghai

5, What is your Main exporting countries?
européen, Moyen-Orient, Amérique du Sud, Southeast Asia market are our main market

Informations Complémentaires

Lieu d'origine:

Chine

Taper:

Nickel Bar

Application:

high temperature

Noter:

Inconel Alloy 625

Ni (Min):

70%

Powder Or Not:

Not Powder

Ultimate Strength (≥ MPa):

80,000 psi (550 MPa)

Elongation (≥ %):

14,000 (965 MPa) 30 (min)

Numéro de modèle:

Inconel Alloy 625

Marque:

fushun

Similar grades:

2.4856